Hi Everyone...

I started building this, past 6 month ago..the issues is hard getting Gordon Glass, Bearpaw glass or other bow backing products in my country...online purchase its not solving whole issues when your local customer wants good bows with cheap cost  ..

In here..Local Handmade traditional bows sale about $ 150 - 200...Imported products sale about $ 350 - 600

So i started to make my own fiberglass to reduce production cost..this simple fiberglass making based on Poltrusion procces..but still homemade    :D    

Molding, lenght 1 meter, width 4,5 cm, depth 1 cm



Moulding Tensioner



Arrange 3 cm nails  
4 pcs Horizontal, 5 pcs vertical




Put mold release wax on main surface and side


I use unidirectional fiber roving like this


Getting started put roving on the mold


After 20 min works


 

andrianyuga

1. Clear Resin ( local common name Resin CMX type )
2. Catalyst
3. Styrene monomer
4. Grooving tools

Mixing Ratio :

- Half cup of glass ( 120 ml )
- 1 table spoon styrene
- 5 - 6 drops catalyst

based from above..you able to works 2 fiberglass strips




After Mixed



Work first inner of roving layer, to avoid dry spot..dont forget to loose molding tension before





And then, pour the resin outer roving surface


Grooving with 1 hour working time before resin getting cured


and after it..make sure there's no dry spot or bubble trap


To avoid resin waste left on the mold, i use hairdryer and grooving with flat surface tool, look at resin waste on top

Buemaker

Very interesting. Let us see the rest.

Mad Max

I would rather fail at something above my means, than to succeed at something  beneath my means  
}}}}===============>>

mwosborn

Wow.  Makes me grateful that my glass is only one quick click away!
Enjoy the hunt!  - Mitch

Roy from Pa

Yup, I get all my glass from Mr. McKenzie.

Bvas

QuoteOriginally posted by Roy from Pa:
Yup, I get all my glass from Mr. McKenzie.
What the????
Some hunt to survive; some survive to hunt

macbow

WoW,, good work.

Roy has been into glass for a long time.  Longnecks.
United Bowhunters of Mo
Comptons
PBS
NRA
VET
"A man shares his Buffalo". Ed Pitchkites

monterey

QuoteOriginally posted by macbow:
WoW,, good work.

Roy has been into glass for a long time.  Longnecks.
:biglaugh:     :laughing:    :laughing:
Monterey

"I didn't say all that stuff". - Confucius........and Yogi Berra

andrianyuga

I put the pressure board on top, and pressed with inner tube band, and tighten the tensioner before
Let it dry in direct sunlight for 4 - 6 hours




during drying procces, you can see resin waste squeezing out


open the pressure board carefully, actually there's no little black spot on it, that's my camera    :D


Cut here


carefully released from the mold



And the results of homemade fiberglass Lam



Holm-Made

Amazing.  

Once the word gets out n this Ol' Kenny will be looking for new employment again.  LOL

andrianyuga

Here's the Bows





Black glass on Tatar Bows


White Glass on Turkish Bows


Clear on One piece recurve


Roy from Pa


Robertfishes

Very nice bows, thanks for sharing the pictures of your fiberglass production.

rainman

Very informative, and imaginative.
Semper Fidelis
Dan Raney

monterey

Very interesting and intriguing. Now I'll end up tripling my glass cost trying to make it.   :biglaugh:
Monterey

"I didn't say all that stuff". - Confucius........and Yogi Berra

bjansen

I am very impressed   Great job

Pretty cool technique you have got there...  Nice looking bows also...

andrianyuga

QuoteOriginally posted by Roy from Pa:
Nice work.

All right Mac, LOL.
thanks..   :D

andrianyuga

QuoteOriginally posted by Shredd:
Pretty cool technique you have got there...  Nice looking bows also...
thikness result is 1.4 mm..must be into drum sander to get 1.2 mm or 1 mm

Contact Us | Trad Gang.com © | User Agreement

Copyright 2003 thru 2025 ~ Trad Gang.com ©