EA-40™
EA-40™
*NOTE: Product Packaging May Vary
EA-40™ Clear Amber Epoxy is an unfilled low-viscosity epoxy adhesive that can be spread easily in thin films that are almost transparent after curing. EA-40™ has a long pot life and cures in 24 hours at room temperature to provide good mechanical and electrical properties. Mix ratio is 1:1 by volume. When mixed 2A:1B by volume, EA-40™ will achieve greater heat resistance and improved physical properties. EA-40™ is versatile and can be used for many different assembly and repair applications ranging from electrical potting to jewelry assembly to repairing plumbing fixtures. Bow makers have come to know EA-40™ as a tremendous laminating resin. EA-40™ provides highly moisture resistant bonds meeting the performance requirements for Federal Specification MMM-A-188, Type III.

I've used it for years on my wood bows and cure it at 85 degrees over night and never had a failure of the glue joint.
I'd imagine the glass bow guys like a little hotter temps though.
#92
The Bowyer's Bench / Re: Crooked Stic-- Best of luc...
Last post by dbeaver - April 13, 2025, 06:28:59 AM
we all thought his handle had to do with bows! After surgery ill be calling you Straight Stick Mike, good luck with everything.
#93
The Bowyer's Bench / Re: Now that’s a gap
Last post by Buemaker - April 13, 2025, 06:09:12 AM
First I thought you had lost your lighter or something. One time we glued a pack of tobacco under vinyl flooring,was in a hurry,had  to rip it off  :banghead:
#94
The Bowyer's Bench / Re: G10
Last post by Buemaker - April 13, 2025, 06:04:03 AM
Looks like some serious tough stuff.
#95
The Bowyer's Bench / Re: 2025 Bow Swap Progress Thr...
Last post by Buemaker - April 13, 2025, 06:02:28 AM
I have never heated Smooth On to more than 125-130 F and have never used that gradual thing.
#96
The Bowyer's Bench / Re: Crooked Stic-- Best of luc...
Last post by Buemaker - April 13, 2025, 05:54:40 AM
Lykke til med operasjonen. :pray:
#97
The Bowyer's Bench / Crooked Stic-- Best of luck wi...
Last post by Roy from Pa - April 13, 2025, 05:41:31 AM
Mike, wishing you the very best with the surgery tomorrow and a speedy recovery...

:pray: :pray:
#98
The Bowyer's Bench / Re: 2025 Bow Swap Progress Thr...
Last post by Crooked Stic - April 12, 2025, 10:54:47 PM
Never have done that. But do what you feel comfortable with.
#99
The Bowyer's Bench / Re: 2025 Bow Swap Progress Thr...
Last post by Watsonjay - April 12, 2025, 10:50:39 PM
Quote from: Watsonjay on April 12, 2025, 10:28:44 PM
I was just reading the ea-40 directions and it said to do a graduated increase in temp. Didn't follow to exactly as it said to take to 185. In dont think any of us do that.
#100
The Bowyer's Bench / Re: 2025 Bow Swap Progress Thr...
Last post by Watsonjay - April 12, 2025, 10:28:44 PM
I was just reading the ea-40 directions and it said to do a graduated increase in temp.