Trad Gang

Main Boards => The Bowyer's Bench => Topic started by: PopeandYoung_51 on February 20, 2017, 11:53:00 PM

Title: What Grits for Drum Sanding Lams (Boo and Veneers)?
Post by: PopeandYoung_51 on February 20, 2017, 11:53:00 PM
What grits do bowyers use for sanding lams down to desired thicknesses?
Title: Re: What Grits for Drum Sanding Lams (Boo and Veneers)?
Post by: Roy from Pa on February 21, 2017, 03:57:00 AM
36 to 60.
Title: Re: What Grits for Drum Sanding Lams (Boo and Veneers)?
Post by: kennym on February 21, 2017, 06:58:00 AM
I usually run 50, the 36 will show sanding marks thru glass in some veneers.
Title: Re: What Grits for Drum Sanding Lams (Boo and Veneers)?
Post by: Mad Max on February 21, 2017, 08:57:00 AM
QuoteOriginally posted by Roy from Pa:
36 to 60.
Us 2 old fart's agree.

I use 60 on all glass bows
Title: Re: What Grits for Drum Sanding Lams (Boo and Veneers)?
Post by: Roy from Pa on February 21, 2017, 09:00:00 AM
I always use 60, but I only make all wood bows. I do know some guys use 36.

Maxi you are right about one thing.

2 old farts.. LOL