What thickness does everyone use.All I can find is 1/16" and appears to be a lot thicker than the old over lays.Anyone know were I can get some about .030 thick.
I just sand then down to desired thickness. Works good for glass, have not tried micarta.
Micarta sands just like glass does. Someone here sells micarta in paper thicknesses unless I am mistaken-anybody know who?
You can also use CORE-TUFF from gordon glass. it is 030 and comes in red and white and black(i think)
Thanks for the responses everyone.I thought about sanding it,but keeping the thickness uniform I was worried about.Bjorn was it Kirk that was making tip material that Bow Doc was testing.Thanks Chuck,I found a supplier for the core tuff.
I used phenbolic on the tips,may try sanding a piece to see how it turns out.Thanks for the help everyone. Terry